What grit removes oxidation from aluminum?
Aluminum has dull oxidation that does not come off with cleaning alone. Recommended grit: Use 320 or 400 for oxidation, then 600, 800, and 1000 for finer prep.
aluminum
oxidation removal
View solution
What grit for aluminum wheel polishing prep?
Aluminum wheels can stay scratched or dull after sanding. Recommended grit: Use 400 or 600 for prep, then 800, 1000, 1500, 2000, and 3000 before polishing.
aluminum
polishing prep
View solution
What grit for cast aluminum?
Cast aluminum can remain rough or show uneven sanding marks. Recommended grit: Use 180 or 220 for rough cast texture, then 320, 400, 600, and 800.
cast aluminum
surface prep